Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.00 g/cc | 0.145 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 202 Aluminum Oxide REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa.. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | calculated from bulk density after subtracting pore volume |
MarkeTech Repton 214 Aluminum Oxide Brand 214 features: High porosity and purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even wh.. |
|||
Density | 4.00 - 4.80 g/cc | 0.145 - 0.173 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 518.002 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 4.00 - 4.80 g/cc | 0.145 - 0.173 lb/in³ | ASTM B417 |
H.C. Starck Amperit® 518.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO) |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | |
Schott N-SF66 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific) LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6 LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6 4.0 specific gravity, Nylon 6 |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | Fiber Density |
Zircar Ceramics ALBF Alumina Bulk Fiber Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give .. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | |
Zircar Ceramics HR-1 Dense Aluminum Oxide Hangar Rod ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth.. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | |
Zircar Ceramics HR-2 Dense Aluminum Oxide Hangar Rod ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth.. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | |
Zircar Ceramics HR-3A Dense Aluminum Oxide Support Rod ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth.. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | |
American Elements A-MITE™ Aluminum Oxide Nanopowder General DescriptionApplicationsA-MITE™ powders and dispersions are recently developed inorganic aluminium oxide nanoparticles with unique abrasion resistance properties for use in optical lenses, w.. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | ISO 1183 |
Eurostar Staramide 6 80E10 PA6, Injection Molded Staramide 6 80E10 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E10)Information provided by Eurostar. |
|||
Density | 4.00 g/cc | 0.145 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec 433 Alumina, 99.9% 433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A .. |