Physical Properties Metric English Comments
Density 4.00 g/cc
0.145 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton 202 Aluminum Oxide
REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even when thermal cycled many times. They are availa..
Density 4.00 g/cc
0.145 lb/in³
calculated from bulk density after subtracting pore volume
MarkeTech Repton 214 Aluminum Oxide
Brand 214 features: High porosity and purity.REPTON setter tiles, kiln furniture, and special fixtures are lightweight, ridge, and high strength ceramics that resist distortion and spalling, even wh..
Density 4.00 - 4.80 g/cc
0.145 - 0.173 lb/in³
ASTM B212
H.C. Starck Amperit® 518.002 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density 4.00 - 4.80 g/cc
0.145 - 0.173 lb/in³
ASTM B417
H.C. Starck Amperit® 518.059 Agglomerated, Sintered Tungsten Carbide-Cobalt 88-12 (WC-CO)
Density 4.00 g/cc
0.145 lb/in³
Schott N-SF66 Glass
Information Provided by SCHOTT North America, Inc.
Density 4.00 g/cc
0.145 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP (Asia Pacific)
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Density 4.00 g/cc
0.145 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Density 4.00 g/cc
0.145 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Density 4.00 g/cc
0.145 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6
Density 4.00 g/cc
0.145 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6
Density 4.02 g/cc
0.145 lb/in³
Schott N-LAK34 Glass
Information Provided by SCHOTT North America, Inc.
Density 4.00 g/cc
0.145 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP AH0400A ABS
LNP* THERMOCOMP* AH0400A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity.
Density 4.00 g/cc
0.145 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP MH0400A PP
LNP THERMOCOMP* MH0400A is a compound based on Polypropylene resin. Added features of this material include: High Specific Gravity.
Density 4.01 g/cc
0.145 lb/in³
DIN EN 623-2
CeramTec DN 70 Dispersion Ceramic, Al2O3-ZrO2
DN 70 is a ZTA Alumina Toughened Zirconia.
Density 4.00 g/cc
0.145 lb/in³
Fiber Density
Zircar Ceramics ALBF Alumina Bulk Fiber
Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give ..
Density 4.00 g/cc
0.145 lb/in³
Zircar Ceramics HR-1 Dense Aluminum Oxide Hangar Rod
ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth..
Density 4.00 g/cc
0.145 lb/in³
Zircar Ceramics HR-2 Dense Aluminum Oxide Hangar Rod
ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth..
Density 4.00 g/cc
0.145 lb/in³
Zircar Ceramics HR-3A Dense Aluminum Oxide Support Rod
ZIRCAR Insulation Hanger and Support Rods are high stability dense aluminum oxide components used to support the roof and walls in ZIRCAR Insulation Assemblies and Furnace Insulation Modules. Togeth..
Density 4.00 g/cc
0.145 lb/in³
American Elements A-MITE™ Aluminum Oxide Nanopowder
General DescriptionApplicationsA-MITE™ powders and dispersions are recently developed inorganic aluminium oxide nanoparticles with unique abrasion resistance properties for use in optical lenses, w..
Density 4.00 g/cc
0.145 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
CeramTec 192/193 Titania
192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra..
Density 4.00 g/cc
0.145 lb/in³
ISO 1183
Eurostar Staramide 6 80E10 PA6, Injection Molded
Staramide 6 80E10 is a high density, Polyamide 6, Injection Molding Resin (also known as 680E10)Information provided by Eurostar.
Density 4.00 g/cc
0.145 lb/in³
DIN EN 623-2 / ASTM-C373 / ASTM-C20
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..