LATI Laticonther 47/1 CP/80 PP Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer LATI
Trade Name Laticonther
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Laticonther 47/1 CP/80 PP Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High thermal conductivity product based on Polypropylene copolymer (PPc). Special filler. Extrusion and molding injection grade.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 2.77 g/cc
0.100 lb/in³
Linear Mold Shrinkage, Flow 0.0075 - 0.0125 cm/cm
0.0075 - 0.0125 in/in
Linear Mold Shrinkage, Transverse 0.0070 - 0.012 cm/cm
0.0070 - 0.012 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
Elongation at Break 40 %
40 %
Tensile Modulus 1.50 GPa
218 ksi
Charpy Impact Unnotched NB
NB
Charpy Impact, Notched 5.00 J/cm²
23.8 ft-lb/in²
Thermal Properties Metric English Comments
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Longitudinal
Deflection Temperature at 0.46 MPa (66 psi) 145 °C
293 °F
Deflection Temperature at 1.8 MPa (264 psi) 140 °C
284 °F
Vicat Softening Point 145 °C

@Load 5.00 kg
293 °F

@Load 11.0 lb
Electrical Properties Metric English Comments
Surface Resistance 1.00e+11 ohm
1.00e+11 ohm
Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Drying Temperature 80.0 - 90.0 °C

@Time 10800 sec
176 - 194 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa