Superior Die Set FORTAL® HP Aluminum Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy
Manufacturer Superior Die Set
Trade Name Fortal®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Superior Die Set FORTAL® HP Aluminum Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: FORTAL is a high strength, lightweight, easy to machine alloy, originally developed to be used in the aerospace industry. It can be found whenever a structure is highly solicited and doesn't require a very high ratio of resistance/mass. FORTAL offers machinability, high resistance to corrosion, and leads to increased productivity. FORTAL's modulus of elasticity is one third that of steel, and can absorb three times as much shock and vibration in its elastic phase. FORTAL is solution heat-treated, stabilized, artificially aged and stress relieved by stretching. Application: FORTAL is an ideal material for all types of products and tooling since it is stronger than 1020 steels.Information provided by Superior Die Set.
Physical Properties Metric English Comments
Density 2.77 g/cc
0.100 lb/in³
Thickness 102000 - 202000 microns
4020 - 7950 mil
intermediate sizes also available
Mechanical Properties Metric English Comments
Hardness, Brinell 145
145
150
150
Tensile Strength, Ultimate 510 MPa
74000 psi
Tensile Strength, Yield 440 MPa
63800 psi
Modulus of Elasticity 71.0 GPa
10300 ksi
Shear Strength 331 MPa
48000 psi
Thermal Properties Metric English Comments
CTE, linear 23.00 µm/m-°C

@Temperature 20.0 - 100 °C
12.78 µin/in-°F

@Temperature 68.0 - 212 °F
Specific Heat Capacity 0.958 J/g-°C
0.229 BTU/lb-°F
Thermal Conductivity 160 W/m-K
1110 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Aluminum, Al 90.07 %
90.07 %
Chromium, Cr 0.23 %
0.23 %
Copper, Cu 1.6 %
1.6 %
Magnesium, Mg 2.5 %
2.5 %
Zinc, Zn 5.6 %
5.6 %