Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.20 g/cc | 0.0795 lb/in³ | Green |
Nabaltec NABALOX® NO 613-10 Reactive Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP KONDUIT OTF2B PPS - Linear LNP KONDUIT* OTF2B is a compound based on PPS - Linear resin containing 10% Glass Fiber, 55% Proprietary Thermal Filler. Added features of this material include: Thermally Conductive. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
LNP Konduit® OTF-212-11 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D4894 |
3M Dyneon™ CC603 PTFE, 15% Fiberglass Filled
(discontinued **) Product Form: White, pelletized free-flowing powder. Applications include bearings, valve seats, seals.Data provided by Dyneon. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Ferro IX 2693 Dental Glass Glass Type: Fused Silica Typical Application: Low Expansion Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also m.. |
|||
Density | 2.20 - 2.30 g/cc | 0.0795 - 0.0831 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G418 Polytetrafluoroethylene 15% Glass Fiber, 5% Molybdenum Disulfide PTFE G Special Compound with glass fiber and molybdenum disulphiteInformation provided by Guarniflon® |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ASTM D792 |
Guarniflon SC 1100 Polytetrafluoroethylene Seal SC series is a superior and unique material for gasket (flat Sealing) applications. The overall benefits of Guarniflon SC series over that of both conventional PTFE and competitive PTFE/filler blen.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0179 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0179 beads include: calibration, high temperature spacer material for gauge control,.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0186 Borosilicate Glass Spheres Appearance: Solid clear borosilicate glass microspheres with white color in powder form.Typical applications of GL0186 beads include: high temperature spacer material for gauge control, coating, fil.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Mo-Sci Corporation GL-0201 Silica Glass Spheres Appearance: Solid clear amorphous silica microspheres with white color in powder form.Typical applications of GL0201 beads include: calibration, high temperature spacer material for gauge control, c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P1 Acid Vapor Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P4 Nitrogen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | theoretical |
Gwent Electronic Materials P2121112P6 Oxygen Plasma Modified Graphene Nanoplatelets Production Method: Plasma Exfoliation of Natural GraphiteColor: Black/Grey Trial product which has not yet been extensively tested.Information provided by Gwent Electronic Materials Ltd. |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 827.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.50 g/cc | 0.0795 - 0.0903 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 827.7 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 - 2.60 g/cc | 0.0795 - 0.0939 lb/in³ | ASTM B212 |
H.C. Starck Amperit® 832.054 Zirconium Oxide-Yttrium Oxide 93-7 (ZrO2-Y2O3) |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
SGL Carbon Group EK 3245 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Saint-Gobain Vitreosil® CFQ/TSC Optical Fused Quartz Vitreosil® CFQ/TSC grades are for use in less demanding applications including viewing windows for use in corrosive and high temperature environments and non-optical components such as spacers, i.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | DIN EN 623-2 / ASTM-C373 / ASTM-C20 |
CeramTec Sikor® S Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
Polyram Metal Cap PPC371B73 Heavy Density Polypropylene, 73% Mineral Filled 73% Mineral filled, heavy density polypropylene copolymer for injection molding metalized part and galvanized covers.Information provided by Polyram. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | Cured |
Chesterton ARC 897 Fine Grade Sliding Wear Compound Description: ARC 897 is an advanced ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It is applied at a t.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Corning Vycor® 7907 UV-Blocking Glass Vycor-UV™ is cerium-doped and provides homogeneous absorption of UV-B and UV-C.Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to hi.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | |
Brandenburger BL 70 Slide Bearing Material BL 70 is a low friction material that exhibits stability at high temperatures. Its applications include high-load low friction tracks and linings in transport and conveying systems, high-stressed b.. |
|||
Density | 2.20 - 2.40 g/cc | 0.0795 - 0.0867 lb/in³ | |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
LNP Konduit® OTF-212-11 BK8-115 Polyphenylene Sulfide, Proprietary Filler
(discontinued **) Features: Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades ar.. |
|||
Density | 2.20 g/cc | 0.0795 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PH0220AC PA 6 (Europe-Africa-Middle East) LNP* Thermocomp* PH0220AC is a compound based on Nylon 6 resin containing High Specific Gravity Filler. |