Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.20 - 2.16 g/cc | 0.0434 - 0.0780 lb/in³ | Average value: 2.03 g/cc Grade Count:22 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc.. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re.. |
|||
Density | 1.96 - 2.16 g/cc | 0.0708 - 0.0780 lb/in³ | Molded |
Bulk Molding Compounds BMC T9 General Purpose Molding Compound BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9.. |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D1050-68 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Density | 2.11 - 2.16 g/cc | 0.0762 - 0.0780 lb/in³ | ASTM D1050-68 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |