Physical Properties Metric English Comments
Density 1.20 - 2.16 g/cc
0.0434 - 0.0780 lb/in³
Average value: 2.03 g/cc Grade Count:22
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Density 2.11 - 2.16 g/cc
0.0762 - 0.0780 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer
Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s..
Density 2.11 - 2.16 g/cc
0.0762 - 0.0780 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® MFA® F1530 Perfluoropolymer
Hyflon® MFA is a family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistanc..
Density 2.11 - 2.16 g/cc
0.0762 - 0.0780 lb/in³
ASTM D792
Solvay Specialty Polymers Hyflon® MFA® F1540 Perfluoropolymer
Hyflon® MFA is a unique family of perfluoro polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame re..
Density 1.96 - 2.16 g/cc
0.0708 - 0.0780 lb/in³
Molded
Bulk Molding Compounds BMC T9 General Purpose Molding Compound
BMC T9 is a low cost, general purpose bulk molding compound designed for the electrical industry. It is UL listed and is used extensively in the manufacture of residential circuit breakers. BMC T9..
Density 2.11 - 2.16 g/cc
0.0762 - 0.0780 lb/in³
ASTM D1050-68
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
Density 2.11 - 2.16 g/cc
0.0762 - 0.0780 lb/in³
ASTM D1050-68
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group