Material Notes:
Information provided by China Tungsten
Physical Properties Metric English Comments
Bulk Density 3.00 g/cc
0.108 lb/in³
Scott
Density 14.4 g/cc
0.520 lb/in³
Binder 2.0
2.0
wax
Particle Size 0.80 µm
0.80 µm
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91
91
Tensile Strength, Ultimate 2200 MPa
319000 psi
Component Elements Properties Metric English Comments
Cobalt, Co 11 %
11 %
Other 0.20 %
0.20 %
WC 88.8 %
88.8 %
Descriptive Properties Value Comments
Flow Rate; sec/50g 31