Material Notes:
Developed as an electrode material, this alloy is used for spark erosion electrodes and contacts giving excellent resistance to mechanical wear and electrical erosion.Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 14.4 g/cc
0.520 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 600 MPa
87000 psi
Thermal Properties Metric English Comments
CTE, linear 10.5 µm/m-°C

@Temperature 20.0 °C
5.83 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.210 J/g-°C
0.0502 BTU/lb-°F
Thermal Conductivity 198 W/m-K
1370 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Copper, Cu 28 %
28 %
Tungsten, W 72 %
72 %