Material Notes:
Optimum wear resistance, high bending strength and high resistance to bonding . Machining of refractory alloys, stainless steel and high manganese steel, etc.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 14.4 g/cc
0.520 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91.5
91.5
Flexural Strength 2100 MPa
305000 psi