Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.47 - 1.76 g/cc | 0.0531 - 0.0636 lb/in³ | Average value: 1.62 g/cc Grade Count:36 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Density | 1.60 - 1.76 g/cc | 0.0579 - 0.0637 lb/in³ | |
Saint-Gobain Chemfab® SlipGrip™ 3 PTFE/Silicone Coated Fiberglass Fabric Description: SlipGrip™ products are PTFE-coated fiberglass fabrics with silicone rubber on one face. This unique combination provides a "slippery" PTFE surface and a "grippy" silicone surface. .. |
|||
Density | 1.70 - 1.76 g/cc | 0.0614 - 0.0636 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Density | 1.46 - 1.76 g/cc | 0.0527 - 0.0636 lb/in³ | Average value: 1.62 g/cc Grade Count:23 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |
|||
Density | 1.36 - 1.76 g/cc | 0.0493 - 0.0636 lb/in³ | Average value: 1.56 g/cc Grade Count:77 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Density | 1.22 - 1.76 g/cc | 0.0439 - 0.0636 lb/in³ | Average value: 1.49 g/cc Grade Count:43 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |