Physical Properties Metric English Comments
Density 1.47 - 1.76 g/cc
0.0531 - 0.0636 lb/in³
Average value: 1.62 g/cc Grade Count:36
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Density 1.70 - 1.76 g/cc
0.0614 - 0.0636 lb/in³
Molding; IS 867-1963
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded
Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit..
Density 1.46 - 1.76 g/cc
0.0527 - 0.0636 lb/in³
Average value: 1.62 g/cc Grade Count:23
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..
Density 1.36 - 1.76 g/cc
0.0493 - 0.0636 lb/in³
Average value: 1.56 g/cc Grade Count:77
Overview of materials for PBT + PET Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of ..
Density 1.22 - 1.76 g/cc
0.0439 - 0.0636 lb/in³
Average value: 1.49 g/cc Grade Count:43
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported..