Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Trilliant™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of competition. When specified, Trilliant® compound may incorporate agency rated materials that meet USP Class IV, FDA or ISO 10993 testing requirements. This Trilliant® grade is a high density specialty compound featuring a sustainable material solution for radiation shielding and weighting & balancing applications. The composite material offers a high performance thermoplastic-based alternative to lead. This compound has densities similar to traditional metals and provides greater flexibility in design and processing.Shielding properties: Attenuation coefficient at 511 keV = 0.83cm-1 Half Thickness at 511 keV = 0.84cmInformation provided by PolyOne
Physical Properties Metric English Comments
Density 8.00 g/cc
0.289 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0050 - 0.015 cm/cm
0.0050 - 0.015 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
ISO 868
Tensile Strength at Break 3.00 MPa
435 psi
ISO 37
Elongation at Break 200 %
200 %
ISO 37
Compression Set 20 - 30 %

@Temperature 23.0 °C,
Time 259000 sec
20 - 30 %

@Temperature 73.4 °F,
Time 72.0 hour
ISO 815
80 - 90 %

@Temperature 70.0 °C,
Time 79200 sec
80 - 90 %

@Temperature 158 °F,
Time 22.0 hour
ISO 815
Thermal Properties Metric English Comments
Thermal Conductivity 1.00 - 2.00 W/m-K
6.94 - 13.9 BTU-in/hr-ft²-°F
Through Plane; ASTM E1461
Electrical Properties Metric English Comments
Surface Resistance 1.00e+6 - 1.00e+9 ohm
1.00e+6 - 1.00e+9 ohm
IEC 60093
Processing Properties Metric English Comments
Melt Temperature 200 - 220 °C
392 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Appearance Grey
Features High Specific Gravity
Non-Toxic
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Housings
Medical/Healthcare Applications
Radiation Shielding
Weighting & Balancing
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved