Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 4.43 g/cc | 0.160 lb/in³ | |
Kobe Steel KS6-4 Alpha-Beta Titanium Alloy, ASTM Gr. 5, Annealed Nominal Composition: Ti-6 Al-4 V Applications: Aircraft parts, connecting rods, valve spring retainers, structural parts, golf club heads.Features:High strength, excellent balance between strength .. |
|||
Density | 4.44 g/cc | 0.160 lb/in³ | |
Ferro IP 550 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Density | 4.43 g/cc | 0.160 lb/in³ | |
Schott N-LAF36 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.43 g/cc | 0.160 lb/in³ | |
Schott N-LASF40 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.44 g/cc | 0.160 lb/in³ | |
Schott N-LASF44 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Fastener Stock Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of fastener stock; more specific form/thickness entries are also available in MatWeb.Industry Specifications: .. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of rod; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aeros.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod or Thickness, 4.00-6.00 in, Annealed, Per Mil-T-9047G; other specific form/thickness entries .. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet Medium To High Strength General-Purpose Alloy. Tensile property data below is typical of sheet; more specific form/thickness entries are also available in MatWeb.Industry Specifications: USA Aero.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5) Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265 Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Sheet and Plate, 0.025-1.000 in, Annealed, Per ASTM B265; other specific form/thickness entries a.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >0.500-1.000 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >0.500-1.000 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), >1.000-1.500 in, STD, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to >1.000-1.500 in, STD, Per Mil-T-9047G; other specific form/thickness entries are also available i.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >2.000-3.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V-0.1Ru; ASTM Grade 29) Medium To High Strength General-Purpose Alloy. Property data below are typical of Timet® 6-4 ELI (without Ru). The 0.1 Ru ELI variant is used for enhanced corrosion resistance.Data provided by TI.. |
|||
Density | 4.43 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32) High Toughness, Heavy Section Weldable AlloyFeatures: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited f.. |
|||
Density | 4.44 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit.. |
|||
Density | 4.44 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; Medium To High Strength General-Purpose Alloy Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A .. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 1.75 - 2.50 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Annealed; 2.50 - 4.00 in Rod or Thickness; Per ASTM F136) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 6-4 ELI Titanium Alloy (Ti-6Al-4V ELI; ASTM Grade 23) (Solution Treated; 0.025 - 1.000 in Sheet and Plate; Per ASTM B265) Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to this MatWeb entry; other specific form/thickness entries are also available in MatWeb.Features: A.. |
|||
Density | 4.42 g/cc | 0.160 lb/in³ | Typical |
TIMET 6-4 Titanium Alloy (Ti-6Al-4V; ASTM Grade 5), Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G Medium To High Strength General-Purpose Alloy. Minimum tensile property data below are specific to Rod, Square, or Hex, >1.500-2.000 in, Per Mil-T-9047G; other specific form/thickness entries are .. |
|||
Density | 4.43 g/cc | 0.160 lb/in³ | |
ATI Allegheny Ludlum Grade 23 (6-4 ELI) Titanium (UNS R56401) The ELI grade has lower impurity limits than standard titanium 6-4.Uses: applications requiring excellent fracture toughness and fatigue strength, aircraft, structural components, biomedical.Mechani.. |
|||
Density | 4.43 g/cc | 0.160 lb/in³ | |
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Blades, discs, rings, airframe, fasteners, components. Vessels, cases, hubs, forgings. Standard, rotor/premium grades. |
|||
Density | 4.43 g/cc | 0.160 lb/in³ | |
ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical. |
|||
Density | 4.44 g/cc | 0.160 lb/in³ | Typical |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, .. |