ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal

Category Metal , Nonferrous Metal , Titanium Alloy , Alpha/Beta Titanium Alloy
Manufacturer ATI Allvac
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ATI Allvac® 6-4ELI Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Allvac.Applications: Applications requiring excellent fracture toughness and fatigue strength; aircraft, structural components, biomedical.
Physical Properties Metric English Comments
Density 4.43 g/cc
0.160 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 290
290
Estimated from Rockwell C value for Brinell test with 3000 kg load/10 mm diameter ball
Hardness, Knoop 315
315
Estimated from Rockwell C value.
Hardness, Rockwell C 30
30
Hardness, Vickers 304
304
Estimated from Rockwell C value.
Tensile Strength, Ultimate 862 MPa
125000 psi
Tensile Strength, Yield 793 MPa
115000 psi
0.2% Offset
Elongation at Break 10 %
10 %
Reduction of Area 25 %
25 %
Component Elements Properties Metric English Comments
Aluminum, Al 6.0 %
6.0 %
Carbon, C <= 0.10 %
<= 0.10 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe 0.20 %
0.20 %
Nitrogen, N 0.030 %
0.030 %
Oxygen, O <= 0.13 %
<= 0.13 %
Titanium, Ti 90 %
90 %
as balance
Vanadium, V 4.0 %
4.0 %