Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.95 g/cc | 0.107 lb/in³ | after firing to 1093°C |
Pyrotek Pyrocast 92AC Tabular Alumina Based Low Cement Castable Pyrocast 92AC is a tabular alumina based low cement castable, enhanced with non-wetting matrix. The silica-free matrix eliminates the potential for aluminum attack on silica with in the bonding mat.. |
|||
Density | 2.95 g/cc | 0.107 lb/in³ | Apparent |
Gouda Vuurvast AC 80-10 Dense Refractory Brick Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard .. |
|||
Density | 2.95 g/cc | 0.107 lb/in³ | Apparent |
Gouda Vuurvast AC 80-5 Dense Refractory Brick Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from.. |
|||
Density | 2.97 g/cc | 0.107 lb/in³ | |
MMCC Aluminum/SiC 55p Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
Density | 2.95 g/cc | 0.107 lb/in³ | Apparent |
Gouda Vuurvast LP 85 AM Dense Refractory Brick Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad.. |
|||
Density | 2.95 g/cc | 0.107 lb/in³ | Apparent |
Gouda Vuurvast LP 85 M Dense Refractory Brick Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs... |
|||
Density | 2.95 g/cc | 0.107 lb/in³ | |
LATI Larton MDT16-02 PPS Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M.. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | |
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPX-PBT-01055 60% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Filler, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | ASTM C135 |
M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |
|||
Density | 2.95 g/cc | 0.107 lb/in³ | |
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that.. |
|||
Density | >= 2.95 g/cc | >= 0.107 lb/in³ | |
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (.. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | |
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |