Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.96 g/cc | 0.107 lb/in³ | |
LATI Laticonther 83 CP/80 PA12, Impact Modified High thermal conductivity product based on Polyamide 12 (PA12), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | ASTM D792 |
Techmer ES HiFill® TPX-PBT-01055 60% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral Filler, 60% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | ASTM C135 |
M Cubed Technologies MMC-S55 Aluminum alloy-55% SiC Metal Matrix Composite High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co.. |
|||
Density | 2.96 g/cc | 0.107 lb/in³ | |
Ceramic Process Systems AlSiC-10, 54 vol% SiC Aluminum alloy A356.2 used. Hermeticity < 1x109 atm-cc/s He.CPS fabricates AlSiC by preparing an SiC preform which is subsequently infiltrated by molten aluminum metal. After infiltration, compone.. |