Physical Properties Metric English Comments
Density 2.95 g/cc
0.107 lb/in³
after firing to 1093°C
Pyrotek Pyrocast 92AC Tabular Alumina Based Low Cement Castable
Pyrocast 92AC is a tabular alumina based low cement castable, enhanced with non-wetting matrix. The silica-free matrix eliminates the potential for aluminum attack on silica with in the bonding mat..
Density 2.95 g/cc
0.107 lb/in³
Apparent
Gouda Vuurvast AC 80-10 Dense Refractory Brick
Description: This bauxite base brick shows, due to the addition of CR2O3, a very good slag resistance.Remarks: This data represents average values, obtained from samples that were cut from standard ..
Density 2.95 g/cc
0.107 lb/in³
Apparent
Gouda Vuurvast AC 80-5 Dense Refractory Brick
Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from..
Density 2.95 g/cc
0.107 lb/in³
Apparent
Gouda Vuurvast LP 85 AM Dense Refractory Brick
Description: LP 85 AM is a brick based on bauxite with a mullite bond. It is characterized by a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, iron lad..
Density 2.95 g/cc
0.107 lb/in³
Apparent
Gouda Vuurvast LP 85 M Dense Refractory Brick
Description: A bauxite brick with a mullite bond with a very low porosity and a high abrasion- and corrosion resistance. Application: torpedo ladles, outlet cement kilns, electric arc furnace roofs...
Density 2.95 g/cc
0.107 lb/in³
LATI Larton MDT16-02 PPS
Polyphenylene Sulfide (PPS) based compound. Magnetic detectable filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & M..
Density 2.95 g/cc
0.107 lb/in³
Goodfellow Shapal™-M soft Aluminum Nitride (AlN) - Machinable
Shapal-M® soft is a high purity, machinable ceramic with high strength and high thermal conductivity. Although the thermal conductivity is not as high as Aluminum Nitride, it is still 50 times that..
Density >= 2.95 g/cc
>= 0.107 lb/in³
COI Ceramics Sylramic™ Crystalline Silicon Carbide (SiC) Fiber
Description: Sylramic™ SiC fiber is a textile grade continuous tow (yarn) made up of 800 filaments with a denier of 1600. Each filament is 10µm in diameter and is coated with a polyvinyl alcohol (..