Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Gouda Vuurvast AC 80-5 Dense Refractory Brick

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast AC 80-5 Dense Refractory Brick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This Cr2O3 containing brick shows a good slag and abrasion resistance. Application in ZnO furnaces.Remarks: This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Density 2.95 g/cc
0.107 lb/in³
Apparent
Porosity 20 %
20 %
Apparent
Mechanical Properties Metric English Comments
Compressive Strength 65.0 MPa
9430 psi
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.90 W/m-K

@Temperature 1100 °C
13.2 BTU-in/hr-ft²-°F

@Temperature 2010 °F
2.00 W/m-K

@Temperature 650 °C
13.9 BTU-in/hr-ft²-°F

@Temperature 1200 °F
2.20 W/m-K

@Temperature 100 °C
15.3 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1700 °C
3090 °F
>= 1750 °C
>= 3180 °F
Deformation under load - t<sub>a</sub>
Component Elements Properties Metric English Comments
Al2O3 84 %
84 %
Cr2O3 5.0 %
5.0 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 10 %
10 %
Descriptive Properties Value Comments
Segercone 38
Thermal Shock Resistance 30 cycles
DIN 51068
Users viewing this material also viewed the following: