Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.81 g/cc | 0.102 lb/in³ | |
PCC-Advanced Forming Technology 30% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Density | 2.81 g/cc | 0.102 lb/in³ | |
Ferro EG 2705 Glaze and Sealant Glass Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulat.. |
|||
Density | 2.81 g/cc | 0.102 lb/in³ | |
Ferro IX 2405 Dental Glass Glass Type: Sr-Al-B-Si Typical Application: Phase Separated Glass Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro .. |
|||
Density | 2.83 g/cc | 0.102 lb/in³ | |
Schott P-PK53 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Alcoa Toolrite 2011®-T3 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Alcoa Toolrite 2011®-T4 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Alcoa Toolrite 2011®-T8 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Density | 2.81 g/cc | 0.102 lb/in³ | |
Constellium ALPLAN® 7075 High-Strength Rolled Precision Aluminum Plate, Milled Both Sides ALPLAN® 7075 precision plates combine a good dimensional stability with high mechanical strength. Both the outstanding flatness and the low roughness of the surfaces, protected by a plastic film, m.. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |
|||
Density | 2.81 g/cc | 0.102 lb/in³ | |
Constellium Fortal® Aluminum Alloy Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m.. |
|||
Density | 2.83 g/cc | 0.102 lb/in³ | |
COI Ceramics Nextel™ AS-N610 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |
|||
Density | 2.83 g/cc | 0.102 lb/in³ | |
Aleris Hokotol Aluminum Alloy, 200 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Density | 2.83 g/cc | 0.102 lb/in³ | |
Aleris Hokotol Aluminum Alloy, 100 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Density | 2.83 g/cc | 0.102 lb/in³ | |
Aleris Hokotol Aluminum Alloy, 300 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |
|||
Density | 2.83 g/cc | 0.102 lb/in³ | |
Aleris Hokotol Aluminum Alloy, 325 mm Thickness Sample treatment not specified for property data.Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; an.. |