Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.82 g/cc | 0.102 lb/in³ | |
Alcoa Toolrite 2011®-T3 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Alcoa Toolrite 2011®-T4 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = D; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Alcoa Toolrite 2011®-T8 Aluminum Weldability = D; Stress Corrosion Cracking Resistance = B; General Corrosion Resistance = D (A = best; E = worst). General 2011 characteristics and uses: Good machinability, especially free-cutting .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Constellium Alumold® 500 Forged Aluminum Forged thick blocks in Alumold® 500 have been developed to provide high and consistent strength across the thickness, good dimensional stability and excellent machinability, in order to respond to .. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Constellium Alumold® 500 Rolled Aluminum The Alumold® 500 alloy has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important prop.. |
|||
Density | 2.82 g/cc | 0.102 lb/in³ | |
Constellium Certal® SPC Forged Aluminum Certal® SPC forged has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property.. |