Ferro EG 2705 Glaze and Sealant Glass

Category Ceramic , Glass , Glaze
Manufacturer Ferro Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ferro EG 2705 Glaze and Sealant Glass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulating over glazes, binding agents and sealants for a variety of ceramic, metal, glass parts and substrates.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 2.81 g/cc
0.102 lb/in³
Particle Size 5.0 µm
5.0 µm
50% of particles
<= 25 µm
<= 25 µm
Thermal Properties Metric English Comments
CTE, linear 7.50 µm/m-°C
4.17 µin/in-°F
at Set Pt.
6.95 µm/m-°C

@Temperature 260 °C
3.86 µin/in-°F

@Temperature 500 °F
Softening Point 925 °C
1700 °F
Annealing Point 825 °C
1520 °F
Transformation Temperature 800 °C
1470 °F
Processing Properties Metric English Comments
Processing Temperature 1300 °C
2370 °F
Typical Firing Temperature