Material Notes:
Aeroglaze® 9743 is a two-part epoxy primer designed for use on aluminum, metal, and prepared composite surfaces. Aeroglaze 9743 primer/tie-coat can be applied to scuff-sanded urethane top coats and epoxy primers. It is also used as a tie coat between scuff sanded weather worn coatings and new urethane topcoats.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
9700B
1.31 g/cc
0.0473 lb/in³
Mixed
1.43 g/cc
0.0517 lb/in³
9743A
Solids Content 57.7 %
57.7 %
9743A; by volume; ASTM D3278-82
62.7 %
62.7 %
Mixed, by volume; ASTM D3278-82
74 %
74 %
9743A; by weight; ASTM D3278-82
75.2 %
75.2 %
Mixed, by weight; ASTM D3278-82
77.8 %
77.8 %
9700B, by volume; ASTM D3278-82
80.3 %
80.3 %
9700B, by weight; ASTM D3278-82
Volatile Organic Compounds (VOC) Content 180 g/l
180 g/l
9700B; ASTM D3960-89
325 g/l
325 g/l
Mixed; ASTM D3960-89
373 g/l
373 g/l
9743A; ASTM D3960-89
Viscosity Measurement <= 30

@Temperature 25.0 °C
<= 30

@Temperature 77.0 °F
9743A; #4 Ford Cup (seconds); ASTM D1200
<= 40

@Temperature 25.0 °C
<= 40

@Temperature 77.0 °F
Mixed; #4 Ford Cup (seconds); ASTM D1200
61

@Temperature 25.0 °C
61

@Temperature 77.0 °F
9700B; #4 Ford Cup (seconds); ASTM D1200
Thermal Properties Metric English Comments
Flash Point >= 21.7 °C
>= 71.1 °F
9743A; Setaflash, Closed Cup; ASTM D3278-82
>= 26.3 °C
>= 79.3 °F
9700B; Setaflash, Closed Cup; ASTM D3278-82
Processing Properties Metric English Comments
Cure Time >= 300 min

@Temperature 25.0 °C
>= 5.00 hour

@Temperature 77.0 °F
Pot Life 240 min

@Temperature 25.0 °C
240 min

@Temperature 77.0 °F
Shelf Life 6.00 Month

@Temperature 21.0 - 27.0 °C
6.00 Month

@Temperature 69.8 - 80.6 °F
9743A
6.00 Month

@Temperature 21.0 - 27.0 °C
6.00 Month

@Temperature 69.8 - 80.6 °F
9700B
Descriptive Properties Value Comments
Appearance Clear Amber
9700B
Red
Mixed
Red
9743A
Coating Film Dry Weight (gm/ft²/mil) 3.7
Theoretical Coverage (ft²/gallon/mil) 1005.7