Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
dry; ISO 1183
Moisture Absorption 2.35 %
2.35 %
Sim. To ISO 62
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
Sim. To ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
Sim. To ISO 294-4
Mechanical Properties Metric English Comments
Tensile Strength, Yield 80.0 MPa
11600 psi
dry; ISO 527-1/-2
Elongation at Break 7.0 %
7.0 %
dry; ISO 527-1/-2
Tensile Modulus 3.40 GPa
493 ksi
dry; ISO 527-1/-2
Flexural Modulus 3.20 GPa
464 ksi
dry; ISO 178
Charpy Impact, Notched 0.300 J/cm²

@Temperature -30.0 °C
1.43 ft-lb/in²

@Temperature -22.0 °F
dry; ISO 179/1eA
0.400 J/cm²

@Temperature 23.0 °C
1.90 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
44.4 µin/in-°F
dry; ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
50.0 µin/in-°F
dry; ISO 11359-1/-2
Melting Point 295 °C
563 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 190 °C
374 °F
dry; ISO 75-1/-2
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
dry; IEC 60695-11-10
V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
dry; IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+9 ohm-cm
1.00e+9 ohm-cm
cond; IEC 60093
1.00e+15 ohm-cm
1.00e+15 ohm-cm
dry; IEC 60093
Dielectric Strength 25.0 kV/mm
635 kV/in
cond; IEC 60243-1
30.0 kV/mm
762 kV/in
dry; IEC 60243-1