SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON RX05489 PA 66 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* STAT-KON* RX05489 is a compound based on Nylon 66 resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength at Break 171 MPa
24800 psi
ASTM D638
Elongation at Break 2.6 %
2.6 %
ASTM D638
Tensile Modulus 15.31 GPa
2221 ksi
50 mm/min; ASTM D638
Flexural Strength 296 MPa
42900 psi
ASTM D790
Flexural Modulus 14.41 GPa
2090 ksi
ASTM D790
Izod Impact, Notched 1.28 J/cm
2.40 ft-lb/in
ASTM D256
Izod Impact, Unnotched 9.61 J/cm
18.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C

@Thickness 3.20 mm
477 °F

@Thickness 0.126 in
unannealed; ASTM D648
Electrical Properties Metric English Comments
Surface Resistance 1.0 - 6.0 ohm
1.0 - 6.0 ohm
ASTM D257