Physical Properties Metric English Comments
Density 0.801 - 1.36 g/cc
0.0289 - 0.0491 lb/in³
Average value: 1.22 g/cc Grade Count:123
Overview of materials for PVC, Transparent
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M..
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds RST 0447/1 Rigid PVC, Extrusion Lead Free
Extrusion transparent films
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds ART 0665/S Rigid PVC, Atoxic for General Purpose
Injection moulding and blow moulding bottles
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds CTS 84 Flexible PVC, Extrusion Modified with Rubber
Gas pipe covering
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds FR 70/1 Flexible PVC, Insulation
Good flexibility cables
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds GSK 88 Flexible PVC, Injection Molding, Lead Free
Technical items
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds HL 91/1 Flexible PVC, Insulation for High Temperatures
Operating temperature 105°C
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds HL 96 Flexible PVC, Insulation for High Temperatures
Operating temperature 90°C
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds ART 0699 Rigid PVC, Atoxic for General Purpose
Bottles suitable for containing oils
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds ART 20 Rigid PVC, Atoxic for General Purpose
Transparent bottles medium/high antishock
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds ART 20/K1 Rigid PVC, Atoxic for General Purpose
Bottles medium antishock
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds ART 30 Rigid PVC, Atoxic for General Purpose
Transparent bottles very high antishock
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds FRT 95 Flexible PVC, Insulation
Telephone and interphone cables
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds PK 8025 Flexible PVC, Lead Free
Sheat according to norm Fiat type 55251
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Fainplast Compounds PM 100 Flexible PVC, Extrusion
Semi-rigid extrusion
Density 1.34 - 1.36 g/cc

@Temperature 20.0 °C
0.0484 - 0.0491 lb/in³

@Temperature 68.0 °F
Oceanchem Group n-Propyl Bromide (NPB)
Molecular Formula: C3H7BrCas No.: 106-94-5Applications: Solvent for industrial cleaning, organic synthesis, pharmaceutical intermediate.Information Provided by Oceanchem Group
Density 1.21 - 1.36 g/cc
0.0437 - 0.0491 lb/in³
Average value: 1.28 g/cc Grade Count:4
Overview of materials for Acrylic/Polycarbonate Alloy, Carbon Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Carbon Fiber Filler". Each property range of values reported is minimum and..
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1184
Fainplast Compounds KL 95/1 Flexible PVC, Insulation for High Temperatures Lead Free
Automotive cables low thickness
Density 0.600 - 1.36 g/cc
0.0217 - 0.0491 lb/in³
Average value: 1.19 g/cc Grade Count:11
Overview of materials for ABS/PVC Alloy
This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW..