Fainplast Compounds FR 70/1 Flexible PVC, Insulation

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds FR 70/1 Flexible PVC, Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Good flexibility cables
Physical Properties Metric English Comments
Density 1.32 - 1.36 g/cc
0.0477 - 0.0491 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 70 - 74
70 - 74
ISO R 868
Tensile Strength at Break >= 13.0 MPa
>= 1890 psi
ISO R 527
Elongation at Break >= 260 %
>= 260 %
ISO R 527
Thermal Properties Metric English Comments
Brittleness Temperature -35.0 °C
-31.0 °F
Cold Flex; ISO 458/2
Descriptive Properties Value Comments
Thermal Stability (minutes) 80
CEI 20-34/3-2