Physical Properties Metric English Comments
Density 0.940 - 1.30 g/cc

@Temperature 170 - 240 °C
0.0340 - 0.0470 lb/in³

@Temperature 338 - 464 °F
Average value: 1.04 g/cc Grade Count:27
Overview of materials for Polyester Thermoplastic Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values..
Density 1.10 - 1.30 g/cc
0.0397 - 0.0470 lb/in³
Average value: 1.16 g/cc Grade Count:16
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Density 0.960 - 1.30 g/cc
0.0347 - 0.0470 lb/in³
Average value: 1.05 g/cc Grade Count:13
Overview of materials for Polypropylene, Stainless Fiber, EMI
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum valu..
Density 0.100 - 1.30 g/cc
0.00361 - 0.0470 lb/in³
Average value: 0.932 g/cc Grade Count:82
Overview of materials for Styrene/Butadiene/Styrene (SBS)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o..
Density 1.20 - 1.30 g/cc
0.0434 - 0.0470 lb/in³
DIN 53479/A
Stanelco Bioplast® GF 106 Biodegradable Plastic
Bioplast 106 is a versatile soft product, suitable for blown film extrusion of completely biodegradable products. Many customers find it is a natural replacement for LDPE. Made from potato starch m..
Density 1.20 - 1.30 g/cc
0.0434 - 0.0470 lb/in³
FTTC 2443
Formosa Plastics 15.5% Sodium Hypochlorite
Information provided by Formosa Plastics Corporation, USA
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds FR 008 Flexible PVC, Insulation
Insulation
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds GS 65 Flexible PVC, Injection Molding for Footwear
Soles - bottom boots
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds FRT 82 Flexible PVC, Insulation
Telephone cables
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds PK 0111 Flexible PVC, Lead Free
Gas pipe according to DIN 4815
Density 1.10 - 1.30 g/cc
0.0397 - 0.0470 lb/in³
Uncured, Part A
3M Scotch-Weld™ EC-2815 B/A FR Epoxy Adhesive
3M Scotch-Weld Epoxy Adhesive EC-2815 B/A FR is a two-component epoxy adhesive with cure at room temperature or with additional heat to form a tough, impact-resistant bond. It has excellent adhesion..
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds PHS 80/B Flexible PVC, Transparent Extrusion
Pipes low migration
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds PM 7516 Flexible PVC, Lead Free
Various profiles stabilized Ca-Zn
Density 1.26 - 1.30 g/cc
0.0455 - 0.0470 lb/in³
ISO R 1183
Fainplast Compounds CL 0133/R Flexible PVC, Sheathing
General purposes