Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.100 - 1.30 g/cc | 0.00361 - 0.0470 lb/in³ | Average value: 0.932 g/cc Grade Count:82 |
Overview of materials for Styrene/Butadiene/Styrene (SBS) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o.. |
|||
Density | 0.100 g/cc | 0.00361 lb/in³ | typical |
MarkeTech Silica Aerogel Silica aerogels are generally known for being an extremely lightweight transparent solid down to |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLOMER® S-2110 SBS Rubber Foam CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLOMER® S-2110D SBS Rubber Foam CELLOMER® FOAM is non-toxic, contains no heavy metal, PVC-free, chloride-free, light weight, superior-grip in wet & dry, high elasticity & resilience. Can be 100% recycled.Information provided by.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5010 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high.. |
|||
Density | 0.100 - 0.150 g/cc | 0.00361 - 0.00542 lb/in³ | |
Sharadaa Ceramics Resin Bonded Mattresses Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.100 g/cc | 0.00361 lb/in³ | |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Density | 0.100 g/cc | 0.00361 lb/in³ | |
Zircar Ceramics MB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 301/F NR-SBR Foam Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-RS EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-BI EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-KPA 45 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 g/cc | 0.00361 lb/in³ | ASTM D3574 |
3M 4516 Foam Tape Use these tapes to protect products from the elements of destruction. Two different backing/adhesive combinations meet demanding applications requiring gasketing, baffling, cushioning, and insulatio.. |
|||
Density | 0.100 g/cc | 0.00361 lb/in³ | ISO 845 |
BASF Neopolen® P 9280 0.1 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | |
3M K1 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.100 g/cc | 0.00361 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-GR EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Density | 0.100 - 0.140 g/cc | 0.00361 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5110 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high d.. |