Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Forever Plast SPA
Trade Name Namtene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Forever Plast Namtene® 1002 Recycled Pipe Grade HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Namtene® 1002 is used for pipes. It features a lower polypropylene content than standard Namtene®.
Physical Properties Metric English Comments
Density 0.945 - 0.970 g/cc
0.0341 - 0.0350 lb/in³
ASTM D792
Melt Flow 0.20 - 0.40 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.20 - 0.40 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
1.3 - 1.9 g/10 min

@Load 5.00 kg,
Temperature 190 °C
1.3 - 1.9 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Ash >= 1 %
>= 1 %
1 hr; 625°C
Mechanical Properties Metric English Comments
Elongation at Break >= 400 %
>= 400 %
ASTM D638
Tensile Modulus >= 1.00 GPa
>= 145 ksi
ASTM D638
Flexural Modulus >= 0.900 GPa
>= 131 ksi
ASTM D790
Izod Impact, Unnotched >= 2.70 J/cm
>= 5.06 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Color Light Grey, Green, or Black
Form Pellets
PP Content < 4%