ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade)

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Exxon Chemical
Trade Name Jayflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Jayflex™ DIDP (0.2% BPA) Plasticizer (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Europe, Middle East & AfricaInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.964 - 0.969 g/cc
0.0348 - 0.0350 lb/in³
ASTM D4052
Viscosity 112 - 127 cP
112 - 127 cP
ASTM D445
Maximum Moisture Content 0.050
0.050
ISO 12937
Optical Properties Metric English Comments
Refractive Index 1.484 - 1.487
1.484 - 1.487
ASTM D1218
Chemical Properties Metric English Comments
Acid Value <= 0.070
<= 0.070
[mg KOH/g]; ASTM D1045
Descriptive Properties Value Comments
Color <30 Pt-Co
ASTM D5386
Ester Content >99.4%
RPP 201