Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.893 g/cc | 0.0323 lb/in³ | ASTM D792 |
Network Polymers NPP 25-1902 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.895 - 0.915 g/cc | 0.0323 - 0.0331 lb/in³ | Average value: 0.904 g/cc Grade Count:8 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Density | 0.894 g/cc | 0.0323 lb/in³ | ASTM D1505 |
Flint Hills P5M2Z-012 Polypropylene Random Copolymer Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
LyondellBasell DP 8310M Polybutene Key Features: semi-crystalline high ethylene content random copolymerApplications: packaging industry, cast film, FDA acceptableMeets FDA requirements in 21 CFR 177.1570 for direct food contact up t.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
LyondellBasell DP 8510M Polybutene Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
Silon Tabond 5008 Adhesive Resin Tabond 5008 is a chemically modified Polypropylene copolymer. Its functional groups improve considerably the bonding between polar polymers, metals and glass.Characteristics: • Strong adhesion .. |
|||
Density | 0.893 g/cc @Temperature 15.6 °C |
0.0323 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 100 Exxon Aviation Oil Aviation Oil 100, 120 and 20W-50 are non-dispersant, mineral oil-based lubricants for piston engines of commercial, military and private aircraft. They contain very low concentrations of anti-oxid.. |
|||
Density | 0.893 g/cc @Temperature 15.6 °C |
0.0323 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 120 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Density | 0.894 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 40 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | Exxon Method |
ExxonMobil EXACT™ 4150 Plastomer Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film a.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ExxonMobil method |
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin Product Description: Exact 4160 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. These resins are designed for blown film applications requir.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CNT 001W Performance Polyolefin Product Description: High impact, medium melt flow rate copolymer, colored black. Particularly suitable for injection molded automotive interior & exterior applications. Availability: North America .. |
|||
Density | 0.893 g/cc @Temperature 15.6 °C |
0.0323 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 120 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Density | 0.895 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 19M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |
|||
Density | 0.893 g/cc @Temperature 15.6 °C |
0.0323 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Mobil Almo 529 Mobil Almo 500 Series lubricants are premium quality high performance products primarily intended for the lubrication of pneumatically operated rock drills in underground and surface mining operatio.. |
|||
Density | 0.894 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Hydroclear® 460 7 EP gear Oil Description: Conoco Hydroclear EP Gear Oil is a premium extreme-pressure industrial gear lubricant with superior deposit control. Hydroclear EP Gear Oil is specially formulated with proprietary addi.. |
|||
Density | 0.893 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Hydroclear® 460 Multipurpose R&O Oil, AGMA Lubricant No. 7 Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidationinhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear .. |
|||
Density | 0.894 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Inca® 460 Oil, AGMA No. 7 Comp. Description: Conoco Inca Oil is a high-quality compounded lubricant recommended for use in heavily loaded industrial and automotive worm gears and bearings operating at moderate to high temperatures.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Par® 100 Hydraulic Oil Description: Conoco Par Hydraulic Oil is an economical hydraulic oil designed to protect the hydraulic systems of underground mining equipment. It is available in ISO grades 68 and 100 and meets the.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D792A |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Density | 0.893 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Conoco® El Mar® Grade 40 Mid Ash Supreme Oil Conoco® El Mar Mid Ash Supreme is a premium quality, mid-ash, dispersant-detergent gas engine oil designed for use in naturally aspirated and moderately to highly turbocharged 4-stroke cycle natura.. |
|||
Density | 0.893 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Hydroclear® 220 Multi-Way Machine Lubricant Description: Conoco Hydroclear Multi-Way Machine Lubricant is a high-quality, heavy-duty circulating machine tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Multi-.. |
|||
Density | 0.895 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 19M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.895 - 1.48 g/cc | 0.0323 - 0.0535 lb/in³ | Average value: 0.986 g/cc Grade Count:93 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM-D792 |
Braskem CP 284R HECO Polypropylene Heterophasic Copolymer CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and proce.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM-D792 |
Braskem CP 743 HECO Polypropylene Heterophasic Copolymer CP 743 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and a general purpose additive package. CP 743 presents high melt strength, good processability, and.. |