Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Mytex Polymers 8224LW Polypropylene, Non-filled, Compounded

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Mytex Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Mytex Polymers 8224LW Polypropylene, Non-filled, Compounded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Mytex® 8224LW is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
ASTM D792
Melt Flow 25 g/10 min
25 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Instant; ISO 868
Tensile Strength, Yield 20.0 MPa
2900 psi
50 mm/min; ISO 527
Flexural Modulus 1.00 GPa
145 ksi
Tangent; 1.3 mm/min; ISO 178
Izod Impact, Notched (ISO) 16.0 kJ/m²

@Temperature 23.0 °C
7.61 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C
172 °F
ISO 75-1
Users viewing this material also viewed the following: