Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. This resin could be used as an impact booster for compounds. Its applications include: buckets, battery cases, industrial and grocery boxes, lids and caps, and compounds.
Physical Properties Metric English Comments
Density 0.895 g/cc
0.0323 lb/in³
ASTM-D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 53
53
ASTM-D785
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM-D638
Elongation at Yield 6.0 %
6.0 %
ASTM-D638
Flexural Modulus, 1% Secant 900 MPa
131000 psi
ASTM-D790
Izod Impact, Notched 0.670 J/cm

@Temperature -20.0 °C
1.26 ft-lb/in

@Temperature -4.00 °F
ASTM-D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 81.0 °C
178 °F
ASTM-D648
Deflection Temperature at 1.8 MPa (264 psi) 49.0 °C
120 °F
ASTM-D648
Vicat Softening Point 140 °C

@Load 1.02 kg
284 °F

@Load 2.25 lb
ASTM-D1525