Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D792 |
Mytex Polymers 8224LW Polypropylene, Non-filled, Compounded Description: Mytex® 8224LW is a non-filled compounded polypropylene produced for automotive applications.Key Applications: Automotive exteriorInformation provided by Mytex Polymers |
|||
Density | 0.895 - 0.915 g/cc | 0.0323 - 0.0331 lb/in³ | Average value: 0.904 g/cc Grade Count:8 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
LyondellBasell DP 8310M Polybutene Key Features: semi-crystalline high ethylene content random copolymerApplications: packaging industry, cast film, FDA acceptableMeets FDA requirements in 21 CFR 177.1570 for direct food contact up t.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
LyondellBasell DP 8510M Polybutene Key Features: semi-crystalline high ethylene content random copolymer, miscible with polyproylenesApplications: Hot Melt Adhesives, FDA acceptableMeets FDA requirements in 21 CFR 175.105 for indirec.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
Silon Tabond 5008 Adhesive Resin Tabond 5008 is a chemically modified Polypropylene copolymer. Its functional groups improve considerably the bonding between polar polymers, metals and glass.Characteristics: • Strong adhesion .. |
|||
Density | 0.895 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil HD Plus 80W-90 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
Total PPR 8573 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8573 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The low m.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D1505 |
Total PPR 8473 Polypropylene, Film Extrusion Grade Random copolymer heat sealable film gradeColor/Clarity/Impact - FINA 8473 is a low melting, high ethylene random copolymer with improved color, optics and impact properties.Heat Sealable - The very .. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | Exxon Method |
ExxonMobil EXACT™ 4150 Plastomer Product Description: Exact 4150 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4150 is designed for multilayer coextruded cast film a.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ExxonMobil method |
ExxonMobil Exact™ 4151 Ethylene-based Plastomer Resin Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer and multilayer coe.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ExxonMobil Method |
ExxonMobil EXACT™ 4151 Plastomer for Cast Film Product Description: Exact 4151 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. Exact 4151 is designed for both monolayer multilayer coextru.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ExxonMobil method |
ExxonMobil Exact™ 4160 Series Ethylene-based Plastomer Resin Product Description: Exact 4160 is an ethylene-based hexane plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. These resins are designed for blown film applications requir.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CNT 001W Performance Polyolefin Product Description: High impact, medium melt flow rate copolymer, colored black. Particularly suitable for injection molded automotive interior & exterior applications. Availability: North America .. |
|||
Density | 0.895 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 19M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
Dow AFFINITY™ PF 1140 Polyolefin Plastomer AFFINITY® PF 1140 polyolefin plastomer is an ethylene alpha-olefin resin designed for use in a variety of demanding applications including high-speed, form-fill seal products, display films and fre.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
Dow AFFINITY™ SE 1400 Polyolefin Plastomer AFFINITY® SE 1400 polyolefin plastomer is an ethylene octene resin that offers excellent performance for profile extrusion of thick tubes and good melt strength for low shear blow molding. It has e.. |
|||
Density | 0.895 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil HD Plus 80W-90 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
ConocoPhillips Par® 100 Hydraulic Oil Description: Conoco Par Hydraulic Oil is an economical hydraulic oil designed to protect the hydraulic systems of underground mining equipment. It is available in ISO grades 68 and 100 and meets the.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D792A |
Braskem CP 195 Injection Molding Polypropylene Description: CP 195 is a very high melt flow rate heterophasic copolymer developed for high speed injection moulding machines and high productivity thin-walled injection moulded parts. The product f.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM-D792 |
Braskem PCD 0440 HECO Polypropylene Heterophasic Copolymer PCD 0440 is a medium melt flow rate heterophasic copolymer with high impact strength. This resin is designed for steel pipe coating (SPC) and injection molding. Its applications include: automotive.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM-D792 |
Braskem PCD 0810 HECO Polypropylene Heterophasic Copolymer PCD 0810 is a high melt flow rate heterophasic copolymer developed for injection molding applications. The product combines high impact strength and good processability with a fair stiffness level. .. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D792A |
Braskem CP 442 XP Injection Molding Polypropylene Description: CP 442XP is a medium melt flow rate heterophasic copolymer suitable for injection molding applications. The product combines good stiffness with excellent impact resistance even at sub-.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM D792A |
Braskem CP 741 Blow Molding Polypropylene Description: CP 741 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and general purpose additive package. CP 741 presents low odor/taste transfer, high mel.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | |
BASF N-Ethylpiperazine Formula: C6H14N2CAS: 5308-25-8Description: N-Ethylpiperazine is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 1-EthylpiperazinApplications: Intermediate us.. |
|||
Density | 0.895 g/cc @Temperature 15.0 °C |
0.0323 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 19M Mobil DTE 10M Series Mobil DTE 10M Series oils are supreme performance anti-wear hydraulic oils engineered for wide temperature range applications. They exhibit optimum flow characteristics at sub-zero temperatures and .. |
|||
Density | 0.895 - 1.48 g/cc | 0.0323 - 0.0535 lb/in³ | Average value: 0.986 g/cc Grade Count:93 |
Overview of materials for Ethylene Butyl Acrylate This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM-D792 |
Braskem CP 284R HECO Polypropylene Heterophasic Copolymer CP 284R is a heterophasic copolymer designed for injection molding of pails and containers with excellent stiffness/impact strength balance. This resin also exhibits excellent productivity and proce.. |
|||
Density | 0.895 g/cc | 0.0323 lb/in³ | ASTM-D792 |
Braskem CP 743 HECO Polypropylene Heterophasic Copolymer CP 743 is a low melt flow rate heterophasic copolymer. It has broad molecular weight distribution and a general purpose additive package. CP 743 presents high melt strength, good processability, and.. |