ConocoPhillips Hydroclear® 220 Multi-Way Machine Lubricant

Category Fluid , Lubricant
Manufacturer ConocoPhillips
Trade Name Hydroclear®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ConocoPhillips Hydroclear® 220 Multi-Way Machine Lubricant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Conoco Hydroclear Multi-Way Machine Lubricant is a high-quality, heavy-duty circulating machine tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Multi-Way Machine Lubricant is specially formulated with proprietary additive chemistry containing oiliness and tackiness agents and is recommended for use on the plain bearing slideways of lathes, shapers, grinders, milling machines and other machine tools. Hydroclear Multi-Way Machine Lubricant also can be used effectively on the slideways of saws and carriages found in lumber mills. Hydroclear Multi-Way Machine Lubricant has exceptional stick/slip properties to prevent problems during slow-speed operations. Hydroclear Multi-Way Machine Lubricant provides exceptional control of lubricant runoff, excellent adhesion to horizontal and vertical way surfaces, good rust and corrosion protection and wear protection. Hydroclear Multi-Way Machine Lubricant is available in ISO viscosity grades 68 and 220. Hydroclear Multi-Way Machine Lubricant has been tested and formally approved by Cincinnati Milacron in accordance with its Lubricant Specifications.Information provided by ConocoPhillips.
Physical Properties Metric English Comments
Density 0.893 g/cc
0.0323 lb/in³
Viscosity Measurement 105
105
Viscosity Index
Saybolt Viscosity at 100°F 1299 SUS
1299 SUS
Saybolt Viscosity at 210°F 104 SUS
104 SUS
Kinematic Viscosity at 40°C (104°F) 230 cSt
230 cSt
Kinematic Viscosity at 100°C (212°F) 20.7 cSt
20.7 cSt
ASTM Color 4.0
4.0
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
Flash Point 271 °C
520 °F
Descriptive Properties Value Comments
Stick/Slip Ratio 0.6