Physical Properties Metric English Comments
Density 0.0280 g/cc
0.00101 lb/in³
0.5 minute residence time pre-expander
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ..
Density 0.0280 g/cc
0.00101 lb/in³
1.2 minute residence time pre-expander
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry in..
Density 0.0280 g/cc
0.00101 lb/in³
1.2 minute residence time pre-expander
Jackon JACKOCELL® S332 Expanded Polystyrene Packaging and Shape Molding
100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S332 which will lead the industry in..
Density 0.0280 - 0.0380 g/cc
0.00101 - 0.00137 lb/in³
sheet density
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0280 - 0.0400 g/cc
0.00101 - 0.00145 lb/in³
sheet density
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0280 - 0.0400 g/cc
0.00101 - 0.00145 lb/in³
sheet density
Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0280 - 1.10 g/cc
0.00101 - 0.0397 lb/in³
Average value: 0.876 g/cc Grade Count:36
Overview of materials for Polystyrene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Extrusion Grade". Each property range of values reported is minimum and maximum values of a..
Density 0.0280 g/cc
0.00101 lb/in³
DIN EN 1602
BASF Styrodur® 2500 C Extruded Rigid Polystyrene Foam (Europe)
Description: Styrodur C is the green extruded rigid polystyrene foam (XPS) from BASF. As a thermal insulation, it makes a significant contribution to climate protection by reducing CO2 emissions. Th..