Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.00145 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Density range normally used
Polimeri Europa Extir® B 2000 AE Expandable Polystyrene, Fast Molding Flame Retardant
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type B 2000 AE is: Molding, Vacuum.Specific characteristics: ..
Density 0.0230 - 0.0400 g/cc
0.000831 - 0.00145 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form ..
Density 0.0180 - 0.0400 g/cc
0.000650 - 0.00145 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 45B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding of very thin parts (5 mm to 20 mm).Infor..
Density 0.0180 - 0.0400 g/cc
0.000650 - 0.00145 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from ..
Density 0.0190 - 0.0400 g/cc
0.000686 - 0.00145 lb/in³
Pressurized batch pre-foamer; Usual Use
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene  (discontinued **)
Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200..
Density 0.0190 - 0.0400 g/cc
0.000686 - 0.00145 lb/in³
Density range normally used
Polimeri Europa Extir® B 2000 Expandable Polystyrene, Fast Molding  (discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l.Processing technology used for Type B 2000 is: Molding, Vacuum.Specific characteristics: Goo..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Density range normally used
Polimeri Europa Extir® C 2000 Expandable Polystyrene, Fast Molding  (discontinued **)
Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type C 2000 is: Molding, Vacuum.Specific characteristics: Ver..
Density 0.0190 - 0.0400 g/cc
0.000686 - 0.00145 lb/in³
Normal molded density assuming cost optimized selection of processing conditions.
Ineos Nova Styrocell® M742C Expandable Polystyrene
A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma..
Density 0.0240 - 0.0400 g/cc
0.000867 - 0.00145 lb/in³
molding density range
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene
GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOL..
Density 0.0280 - 0.0400 g/cc
0.00101 - 0.00145 lb/in³
sheet density
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0280 - 0.0400 g/cc
0.00101 - 0.00145 lb/in³
sheet density
Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
ISO 845-88
Eurofoam Evacell EVA 30 EVA + PE Foam
Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
ISO 845-88
Eurofoam Polycell PE 30 Polyethylene Foam
Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use..
Density 0.0200 - 0.0400 g/cc
0.000723 - 0.00145 lb/in³
Normal molded density
NOVA Chemicals Styrocell® D733A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol..
Density 0.0240 - 0.0400 g/cc
0.000867 - 0.00145 lb/in³
molding density range
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene
General: Pentfoam 328H is a high density grade expandable polystyrene containing pentane as blowing agent, this grade is developed to meet the demand for fast molding cycles in vacuum machineApplica..
Copyright © lookpolymers.com All Rights Reserved