Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Zotefoams
Trade Name Plastazote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstanding physical attributes.Information provided by Zotefoams
Physical Properties Metric English Comments
Density 0.0280 - 0.0400 g/cc
0.00101 - 0.00145 lb/in³
sheet density
Cell Length 0.150 - 0.500 mm
0.00591 - 0.0197 in