Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Density range normally used |
Polimeri Europa Extir® B 2000 AE Expandable Polystyrene, Fast Molding Flame Retardant Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type B 2000 AE is: Molding, Vacuum.Specific characteristics: .. |
|||
Density | 0.0230 - 0.0400 g/cc | 0.000831 - 0.00145 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form .. |
|||
Density | 0.0180 - 0.0400 g/cc | 0.000650 - 0.00145 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 45B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product allowing to obtain optimum mechanical properties for form molding of very thin parts (5 mm to 20 mm).Infor.. |
|||
Density | 0.0180 - 0.0400 g/cc | 0.000650 - 0.00145 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 45XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for from .. |
|||
Density | 0.0190 - 0.0400 g/cc | 0.000686 - 0.00145 lb/in³ | Pressurized batch pre-foamer; Usual Use |
NOVA Chemicals Gedexcel® 54XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts wit.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Density | 0.0190 - 0.0400 g/cc | 0.000686 - 0.00145 lb/in³ | Density range normally used |
Polimeri Europa Extir® B 2000 Expandable Polystyrene, Fast Molding
(discontinued **) Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 18 g/l.Processing technology used for Type B 2000 is: Molding, Vacuum.Specific characteristics: Goo.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Density range normally used |
Polimeri Europa Extir® C 2000 Expandable Polystyrene, Fast Molding
(discontinued **) Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type C 2000 is: Molding, Vacuum.Specific characteristics: Ver.. |
|||
Density | 0.0190 - 0.0400 g/cc | 0.000686 - 0.00145 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
Ineos Nova Styrocell® M742C Expandable Polystyrene A high strength regular molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for medium density foam.Applications: Styrocell M742C is used ma.. |
|||
Density | 0.0240 - 0.0400 g/cc | 0.000867 - 0.00145 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 455E Expandable Polystyrene GENERAL: PENTFOAM "455E" IS A SELF EXTINGUISHING (SE) GRADE EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST CYCLES IN VACUUM MOL.. |
|||
Density | 0.0280 - 0.0400 g/cc | 0.00101 - 0.00145 lb/in³ | sheet density |
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0280 - 0.0400 g/cc | 0.00101 - 0.00145 lb/in³ | sheet density |
Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 30 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | ISO 845-88 |
Eurofoam Polycell PE 30 Polyethylene Foam Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Normal molded density |
NOVA Chemicals Styrocell® D733A Expandable Polystyrene
(discontinued **) This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for contour molding.Applications: This grade is used for dry mol.. |
|||
Density | 0.0240 - 0.0400 g/cc | 0.000867 - 0.00145 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 328H Expandable Polystyrene General: Pentfoam 328H is a high density grade expandable polystyrene containing pentane as blowing agent, this grade is developed to meet the demand for fast molding cycles in vacuum machineApplica.. |