Physical Properties Metric English Comments
Density 0.300 g/cc
0.0108 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres
EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo..
Density 0.300 - 0.600 g/cc
0.0108 - 0.0217 lb/in³
Sinotek Materials BG Board Ceramic Fiber Board, White, Heat Insulation Material
Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and ..
Density 0.300 - 0.600 g/cc
0.0108 - 0.0217 lb/in³
Sinotek Materials HFB Board Heat Insulation Material Ceramic Fiber Board, White
Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and ..
Density 0.300 - 0.600 g/cc
0.0108 - 0.0217 lb/in³
Sinotek Materials HG Board Heat Insulation Material Ceramic Fiber Board, White
Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i..
Density 0.300 - 0.500 g/cc
0.0108 - 0.0181 lb/in³
Solvay MIRAPOL® SURF-S 410 Surfactant
Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â..
Density 0.300 g/cc
0.0108 lb/in³
Zircar Refractory Composites RS-B ALUMINA-SILICA MOLDABLE
ZIRCAR Alumina-Silica Insulating Blanket Type RS-B Moldable is composed of long, high strength ceramic fibers, with an inorganic alumina binder/rigidizing agent. It is a wet blanket that is shipped ..
Density 0.300 g/cc
0.0108 lb/in³
Cymat A35620SC 030SS Stabilized Aluminum Foam
Description: Cymat A35620SC 030SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.3 g/cm3. The mechanical properties of SAF make it ..
Density 0.300 g/cc
0.0108 lb/in³
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..
Density 0.300 - 0.390 g/cc
0.0108 - 0.0141 lb/in³
Range
3M S38XHS Glass Bubbles
3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik..
Density 0.300 - 0.400 g/cc
0.0108 - 0.0145 lb/in³
DIN 53479 A
BIW ASTM Class 2D2 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...
Density 0.300 - 0.340 g/cc
0.0108 - 0.0123 lb/in³
True, 3M QCM 14.24.6
3M D32/4500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.300 - 0.600 g/cc
0.0108 - 0.0217 lb/in³
Sinotek Materials LG Board Heat Insulation Material Ceramic Fiber Board, White
Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i..
Density 0.300 - 0.600 g/cc
0.0108 - 0.0217 lb/in³
Sinotek Materials PMF Board Heat Insulation Material Ceramic Fiber Board, White