Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.300 - 0.390 g/cc | 0.0108 - 0.0141 lb/in³ | Range |
3M S38XHS Glass Bubbles 3M™ Glass Bubbles S38XHS have a density of .38 g/cc and an isostatic crush strength of 5500 psi with a minimum survival of 90% as compared to S38HS, which has a target 90% survival of 5500 psi. Lik.. |