Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Solvay MIRAPOL® SURF-S 410 Surfactant Description: Granulated rinse aid polymer for use in automatic dish washing powders or tablets. 18% activeIdentification: BLEND OF ACRYLIC BASED POLYMER AND SODIUM TRIPOLYPHOSPHATE.Use level : 0.5 â.. |
|||
Density | 0.350 - 0.500 g/cc | 0.0126 - 0.0181 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D3 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |