Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | ASTM D1505 |
PolyOne Geon™ 120 Series 129 Polyvinyl Chloride Homopolymer The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging.. |
|||
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | ASTM D1505 |
PolyOne Geon™ 170 Series 173 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | ASTM D1505 |
PolyOne Geon™ 170 Series 179 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron®.. |
|||
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | ASTM D1505 |
PolyOne Geon™ 120 Series 121AR Polyvinyl Chloride Homopolymer (PVC Homopolymer) Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Pac.. |
|||
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | Dried Density (Depending on Tamp Density) |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® T22 Tamping Mix Description: THERMOSEAL® T22 FIBERPAK® TAMPING MIX is a wet taping mix made up of bulk refractory fibers and a high temperature binder system. T22 FIBERPAK® TAMPING MIX is particularly good.. |
|||
Density | 0.320 - 0.400 g/cc | 0.0116 - 0.0145 lb/in³ | Dry |
Unifrax Fiberfrax® FC-25 Tamping Mix Casting Mix Fiberfrax FC-25 tamping mix and Vari-Form™ castable materials provide casting mixes which can be applied in small areas such as furnace access and site doors, tube sheets, and as a refractory backu.. |
|||
Density | 0.340 - 0.400 g/cc | 0.0123 - 0.0145 lb/in³ | |
3M K37 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D2 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |
|||
Density | 0.0100 - 0.400 g/cc @Pressure 0.101 MPa, Temperature 20.0 °C |
0.000361 - 0.0145 lb/in³ @Pressure 14.7 psi, Temperature 68.0 °F |
|
BASF Neopolen® P 92HD 105 Expanded Polypropylene (Europe) Description: Neopolen® P 92HD 105 is expanded Polypropylene supplied in the form of beads. The cells are largely closedInformation provided by BASF |