Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.280 - 0.600 g/cc | 0.0101 - 0.0217 lb/in³ | |
FiberNide Nickel Foam Description: Produced in one meter wide continuous sheets in thickness from 1.6 to 2 mm and sold in rolls. Principally used to make the positive plate in nickel metal hydride batteries.Information .. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials BG Board Ceramic Fiber Board, White, Heat Insulation Material Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials HFB Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and .. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials HG Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |
|||
Density | 0.500 - 0.600 g/cc | 0.0181 - 0.0217 lb/in³ | |
BASF Imidazole Formula: C3H4N2CAS: 288-32-4Description: Imidazole is a crystalline powder with an amine-like odor. It is soluble in water.Synonyms: 1,3-Diaza-2,4-cyclopentadiene, 1,3-Diazole, Imidazol, Methanimid.. |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials LG Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |
|||
Density | 0.400 - 0.600 g/cc | 0.0145 - 0.0217 lb/in³ | DIN 53479 A |
BIW ASTM Class 2D4 Silicone Foam Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters... |
|||
Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Sinotek Materials PMF Board Heat Insulation Material Ceramic Fiber Board, White Ceramic Fiber Board is used for the following applications: sealing for furnace doors, thermal and electric insulation for heaters, glass and ceramics, high temperature and thermal insulation, and i.. |