Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.110 - 0.140 g/cc | 0.00397 - 0.00506 lb/in³ | ASTM D792 |
Microcell Composite Company CELLIFF® F7010 Polymer Foam CELLIFF® FOAM is Light & rigid, tenacious & durable. Patterns can be easily molded into the foam surface. We possess the technology to increase surface hardness to meet requirement.Information pr.. |
|||
Density | 0.110 g/cc | 0.00397 lb/in³ | dry |
Microtherm Group MT Thermosphere® Moldable Insulation Paste MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste.. |
|||
Density | 0.110 g/cc | 0.00397 lb/in³ | ASTM D1622 |
SABIC Innovative Plastics ULTEM Foam XP110 PEI ULTEM foam is a polyetherimide based thermoplastic foam with excellent flame, smoke and toxicity performance. The material combines a high strength to weight ratio with low moisture absorption. The .. |
|||
Density | 0.110 g/cc | 0.00397 lb/in³ | ISO 845 |
BASF Neopolen® P 9280 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Density | 0.110 g/cc | 0.00397 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® R82.110 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines outstanding fire resistance with low smoke and toxicity, along with excellent dielectric properties. It has a good strength to .. |
|||
Density | 0.110 g/cc | 0.00397 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® T90.100 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |
|||
Density | 0.110 g/cc | 0.00397 lb/in³ | ISO 845 |
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Density | 0.110 - 0.150 g/cc | 0.00397 - 0.00542 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 B EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |