Polymer Property : Density = 0.000831 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.0230 - 0.0600 g/cc
0.000831 - 0.00217 lb/in³
Pressurized batch pre-foamer; Usual Use
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr..
Density 0.0230 - 0.0400 g/cc
0.000831 - 0.00145 lb/in³
Usual Use
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form ..
Density 0.0230 - 0.0600 g/cc
0.000831 - 0.00217 lb/in³
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene  (discontinued **)
Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi..
Density 0.0230 - 0.0330 g/cc
0.000831 - 0.00119 lb/in³
sheet density
Zotefoams Plastazote® HD30 High Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..