Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0230 - 0.0600 g/cc | 0.000831 - 0.00217 lb/in³ | Pressurized batch pre-foamer; Usual Use |
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr.. |
|||
Density | 0.0230 - 0.0600 g/cc | 0.000831 - 0.00217 lb/in³ | |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Density | 0.0220 - 0.0600 g/cc | 0.000795 - 0.00217 lb/in³ | |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |
|||
Density | 0.0220 - 0.0600 g/cc | 0.000795 - 0.00217 lb/in³ | Density range normally used |
Polimeri Europa Extir® P 1212 Expandable Polystyrene, Special Purpose
(discontinued **) Particle size range is 0.2 - 0.5 mm. Minimum apparent density on a discontinuous pre-expander is 21 g/l. Minimum apparent density on a continuous pre-expander is 25 g/l.Processing technology used .. |
|||
Density | 0.0400 - 0.0600 g/cc | 0.00145 - 0.00217 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 50/S EVA + NR Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |