| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Strength | 310 MPa | 45000 psi | STN EN ISO 178 |
|
Plastcom SLOVAMID® 6/6T GF 35 TS PA6/6T reinforced with glass fiber, improved heat resistance
PA 6/6T for injection molding, reinforced with 35% of glass fiber, for moldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry, improved..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding
43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
PolyOne Nymax™ GF 1200 A 55 HS Black 13 Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ISO 178 |
|
Solvay Specialty Polymers Ixef® 1025 Polyarylamide (PARA)
(Unverified Data**)
Ixef 1025 is a 50% glass-fiber reinforced, UV stabilized polyarylamide which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance. - Black: Ixef 1025/9..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
LNP Stat-Kon® EC-1008 EM BK8-115 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **)
Features: Electrically Conductive, Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; howev..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | |
|
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | |
|
ICE Al2O3 94
Data provided by the manufacturer, International Ceramic Engineering.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | |
|
ICE Al2O3 96
Data provided by the manufacturer, International Ceramic Engineering.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | 5 mm/min; ISO 178 |
|
Gromax BFG45-AS00N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | |
|
Haysite 44500 Vinyl Ester SMC, 30% Glass Reinforced
The 44500 series sheet molding compound offers high strength and excellent resistance to corrosive agents. This compression molding grade is formulated with a vinyl ester resin system.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA), 35% Glass Fiber (Dry)
Amodel® A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high stre..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Techmer ES HiFill® PA6 GF50 IM L NAT001 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricated and Impact ModifiedProcessin..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Techmer ES HiFill® PEEK CF20 TL15 HF 20% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: High Flow and LubricatedInformation provided by TP Composi..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP 9X10312 PA (Asia Pacific)
9X10312 is 50% glass fiber reinforced, impact modified nylon material. High modulus, high flow and good ductility, Low Moisture Absorption.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Techmer ES Electrablend® PA6 CF30 30% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 30% Filler by WeightFeatures: Conductive Appearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Solvay TECHNYL® 2912GMH7-P PA66, 63% glass fiber, DRY
Description: Polyamide 66, reinforced with 63% of glass fiber for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2912GMH7-P is used in all sectors of industry, offerin..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Chase Plastics CP Pryme® NN130GMD2 (DAM) Nylon 66, 30% Glass Fiber Reinforced, 2% MoS2 Lubricated
Information provided by Chase Plastics.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ISO 178-93 |
|
Wellman Wellamid® GFX1717-N1 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66
Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | Elastic Limit in Bending, across direction of rolling |
|
CLAL-MSX CUPROROR® TL5 Spring, Copper Alloy
Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperat..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
Ashley Polymers Ashlene® 528L-50LG Nylon 66, 50% Long Glass Fiber Reinforced
Long glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than available with conventional glass reinforced resins.Data provi..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | |
|
Anderman Ceramics EA96 Sintered Alumina, 96%
High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics.
|
|||
| Flexural Strength | 310 MPa | 45000 psi | 2 [mm/min]; ISO 178 |
|
Akro-Plastic Akromid® S3 GF 50 1 (3533) PA 6.10 Dry, 50% Glass Filled
A characteristic property of AKROMID® S (PA 6.10) is that it has a renewable-resource content of up to 70 % and therefore fulfils the current definition of a bioplastic. The plant-based raw materia..
|
|||
| Flexural Strength | 310 MPa | 45000 psi | ASTM D790 |
|
LNP Thermocomp® UF-1008 Polyphthalamide, Glass Fiber Reinforcement
(discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
|
|||