| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Charpy Impact Unnotched | 1.20 - 1.40 J/cm² | 5.71 - 6.66 ft-lb/in² | Injection and Compression; ISO 179/1eU |
| Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very .. |
|||
| Charpy Impact Unnotched | 1.20 - 1.60 J/cm² @Temperature 23.0 °C |
5.71 - 7.61 ft-lb/in² @Temperature 73.4 °F |
Injection and Compression; ISO 179/ 1eU |
| Raschig Group EPOXIDUR® 3582 EP Epoxy Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi.. |
|||
| Charpy Impact Unnotched | 1.20 - 999.9 J/cm² @Temperature -40.0 - -20.0 °C |
5.71 - 4759 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.71 J/cm² Grade Count:44 |
| Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
| Charpy Impact Unnotched | 1.20 - 1.20 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 5.71 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.20 J/cm² Grade Count:2 |
| Overview of materials for Polyphthalamide (PPA), Aramid Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
|
| Ineos ABS Lustran® QE 1006, Extrusion Grade
(discontinued **) Extrusion grade with high impact.Applications: High impact plates.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majo.. |
|||
| Charpy Impact Unnotched | 1.20 - 1.40 J/cm² | 5.71 - 6.66 ft-lb/in² | Injection; ISO 179/1eU |
| Raschig Group RESINOL® 87120 EPF Phenolic Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets .. |
|||
| Charpy Impact Unnotched | 1.20 - 1.30 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 6.19 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.27 J/cm² Grade Count:4 |
| Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
| Charpy Impact Unnotched | 1.20 - 4.00 J/cm² | 5.71 - 19.0 ft-lb/in² | Average value: 2.33 J/cm² Grade Count:3 |
| Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
| Charpy Impact Unnotched | 1.20 - 1.20 J/cm² @Temperature -40.0 - -20.0 °C |
5.71 - 5.71 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.20 J/cm² Grade Count:1 |
| Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | edgewise; ISO 179 1eU |
| Lehmann & Voss LUVOCOM® 1301-8386 PPS, linear, with aramid reinforcement and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Lehmann & Voss LUVOCOM® 20/AF/15/TF/10 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
| Lehmann & Voss LUVOCOM® 20-7687 Polyphthalamide, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low influence from moisture an.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eU |
| Lucite International Diakon® Frost 902 70 Acrylic Polymer Information provided by Lucite International |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | |
| LATI Latigray 37 B01-01 CX/35 Bio-Polymer Radiopaque compound based on Bio-Polymer (PLA, PHB, ...). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
| Styrolution PS 486N HIPS Styrolution PS 486N is a normal flowing, high impact grade that is especially suitable for blends with a high proportion of general purpose polystyrene (preferably Styrolution PS 165N of Styrolution.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature -20.0 °C |
5.71 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
| Borealis Daplen™ HJ060UB Polypropylene Compound for Direct Left Manufactured Applications Daplen FJ060UB is a special low viscosity compound for direct LFT manufacturing process. It interacts perfectly with glass fibers to create excellent stiffness and impact resistance. Daplen HJ060U.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
| Vyncolit X6151 Novolac Phenolic Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Highest impact, high strain to failure, glycol resistant.USES: Water pumps and water pump .. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
| Vyncolit X680 Novolac Phenolic Glass fiber and glass bead filled phenolic molding compound with excellent mechanical and thermal properties. Easily transformed into complex shapes. UL listed.USES: Complex precision parts with t.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eU |
| Borealis Daplen™ EG102AI Polypropylene Compound 15% Mineral Filled Daplen EF102AI is a 15% mineral filled polypropylene compound intended injection molding. EG102AI is an easy flow grade, specially developed for the car industry. Daplen EF102AI has been developed.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
|
| BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
|
| BASF Novolen® 1100 VC Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eU |
| Hexion Bakelite™ PF 6501 Phenolic Formaldehyde Resin, Low Shrinkage Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistant.Application areas: Thermally and dyna.. |
|||
| Charpy Impact Unnotched | 1.20 - 2.17 J/cm² | 5.71 - 10.3 ft-lb/in² | Average value: 1.57 J/cm² Grade Count:5 |
| Overview of materials for Acrylic, Cast This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 |
| Lucite International Perspex™ GS Acrylic Cast Sheet 000/0000 PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1D |
| Lucite International SW Sanitary Ware Acrylic Sheet Lucite® SW complies with ISO 7823-1 and EN 263. It is approved by the French ARNOR "NF" quality mark.Information provided by Lucite International |
|||
| Charpy Impact Unnotched | 1.20 J/cm² - NB @Temperature -40.0 - 0.000 °C |
5.71 ft-lb/in² - NB @Temperature -40.0 - 32.0 °F |
Average value: 8.38 J/cm² Grade Count:41 |
| Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | edgewise; ISO 179 1eU |
| Lehmann & Voss LUVOCOM® 1301-8291 PPS, linear, with aramid reinforcement Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma.. |
|||
| Charpy Impact Unnotched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eU |
| Lucite International Diakon® Frost 902 80 Acrylic Polymer Information provided by Lucite International |
|||